Code:SUS316L Stainless steel
SUS316 is classified as an austenitic stainless steel (16-18Cr-10-14Ni), and by adding molybdenum (Mo: 2-3%), it has better corrosion resistance than SUS304, even under high concentration of hydrochloric acid solution such as seawater. SUS316L is low carb
| Electrical Resistivity [μΩm] |
Thermal Expansion Coefficient ×10-6/ |
Density g/cm3 (20℃) |
Melting Point ℃ |
|---|---|---|---|
| 0.77 | 16.0 | 7.98 | 1370 |
| Mechanical Properties | Temper | Wire Diameter φmm |
Tensile Strength MPa |
Elongation % |
|---|---|---|---|---|
| W1 (Annealed) | Over 0.05 to 0.16 | 730–980 | ≥20 | |
| Over 0.16 to 0.50 | 680–930 | ≥20 | ||
| Over 0.50 to 1.60 | 650–900 | ≥30 | ||
| W2 (1/2 Hard) | 0.8 to 1.60 | 780–1130 | – | |
| WPB (Hard) | 0.23 to 0.40 | 2050–2300 | – | |
| 0.45 to 0.60 | 1950–2200 | – | ||
| 0.65 to 1.00 | 1850–2100 | – | ||
| 1.20 to 1.40 | 1750–2000 | – | ||
| 1.60 to 2.0 | 1650–1900 | – |
| Chemical Composition |
C | Ni | Cr | Mo | Si | Mn | P | S |
|---|---|---|---|---|---|---|---|---|
| (%) | ≦0.03 | 12.0~15.0 | 16.0~18.0 | 2.0〜3.0 | ≦1.00 | ≦2.00 | ≦0.045 | ≦0.030 |
| Alloys | Type | Diameter (mm) | |
|---|---|---|---|
| SUS316L | Wire | φ6.00~0.020 | |
| SUS316L | Ribbon | t=2.90~0.05 | w=40~0.2 (Depends on thickness) |